The copper sulfate test is used to detect the presence of metallic iron and iron oxide on the surface of materials. Question - What solution strength is needed to copper sulfate solution can be used to determine if a metal is stainless steel or just steel ? Answer - Copper sulfate (CuSO4*5H2O) + H2SO4 (anywhere from 1% to 50% is specified in…

Read full description →

The copper sulfate test is used to detect the presence of metallic iron and iron oxide on the surface of materials.

Question - What solution strength is needed to copper sulfate solution can be used to determine if a metal is stainless steel or just steel ? 
Answer    - Copper sulfate (CuSO4*5H2O) + H2SO4 (anywhere from 1% to 50% is specified in various test methods).





How does copper sulfate test for passivation work?

ANSWER : Chromium and nickel will not be replaced with the Copper sulfate test solution (which also contains sulfuric acid), only the Fe or other less noble metals. If there is free iron on the surface it will be replaced by the copper, forming the distinctive copper color on the surface in this 6 minute test. Of course, this test should only be used on austenitic stainless steel. Some people use it on other grades, but you can get false failures.

 

 

Click here for PASSIVATING LIQUID technical information , to know Other testing methods for PASSIVATION , Passivation Method


Spray the surface with a solution of copper sulfate in water. If free iron is present, a copper film will form. In this test, the chemical reaction is:

 Fe + CuSO4 = FeSO4 + Cu
The copper film is immediately visible.
 

Copper sulphate test: a galvanic type test in which the more noble copper plays upon less noble iron particles but not on SS.  Patches of copper sulphate shows a poorly passivated surface. Passivated parts are immersed in a Copper Sulfate solution for five minutes, rinsed and visually examined. Any copper (pink) color indicates the presence of free iron and the test is considered unacceptable.

Ferroxyl test: causes coloured iron compounds to appear as specks.


Keywords

Supply in Sohar & across Oman

Sohar Chemicals supplies Copper Sulfate LR for passivation test to customers in Sohar, Sohar Port & Freezone, Liwa, Shinas, Saham, Barka, Muscat and across Oman, from our stock in Barka.

Bulk and small orders welcome. Contact us for price, availability, MSDS and TDS.

Need Copper Sulfate LR for passivation test in Sohar?

Get a quick quote with MSDS, packing options and delivery across Sohar and Oman. Bulk and small orders welcome.

About

Sohar Chemicals, part of MBBT Group, is Oman's trusted source for marine and industrial chemicals. We supply high-performance solutions for cleaning, marine, water treatment, and maintenance.

Contact info

Get on time delivery to any port, any city in Oman. We have full inventory of fast running chemicals. Get our quotation by simply sending an email on the below mail id.